ITEM | Standard Number | Descriptions |
1 | SAE AMS 5709H (2008) | Nickel Alloy, Corrosion and Heat-Resistant, Bars and Forgings 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1975°F (1079°C) Solution, Stabilization, and Precipitation Heat Treated |
Elements | Min.(≥) | Max.(≤) |
C | 0.07 | |
Si | 0.10 | |
Mn | 0.10 | |
Cr | 19.75 | |
Ni | remaining | |
Mo | 4.45 | |
Co | 14.00 | |
W | ||
Al | 1.40 | |
Cu | ||
Ti | 3.00 | |
Fe | 0.75 | |
B | 0.005 | |
Zr | 0.04 |