Home»Products > Superalloy > Nimonic 80A / NiCr20TiAl(2.4952) / UNS N07080/ BS 3HR1

Quick Details

GE spec NB 00146, Ideally released to GE spec NB 00146 or to ASTM B637 or WK 2 4952 or BS 3HR1, VIM+ESR, Hot Forging,Polishing,

Delivery

  • Delivery status:Forged 、Solutioned 、
  • Surface:Polished 、
  • Standard:ASTM
  • Shape:Round,Flat,Square,Hexagon,Plate,Sheet,Other

Inventory Status

Order

Nimonic 80A / NiCr20TiAl(2.4952) / UNS N07080/ BS 3HR1Range of products
Product typeProductsDimensionProcesses
Plates/SheetsPlates/Sheets0.08-200mm(T)*W*LForging,hot rolling and cold rolling
Steel BarRound Bar,Flat Bar,Square BarΦ8-1200mm*LForging,hot rolling and cold rolling,Cast
Coil/StripSteel Coil/Steel Strip0.03-16.0x1200mmCold-Rolled&Hot-Rolled
Pipes/TubesSeamless Pipes/Tubes,Welded Pipes/TubesOD:6-219mm x WT:0.5-20.0mmHot extrusion,Cold Drawn,Welded

View chemical composition and mechanical properties of Nimonic 80A / NiCr20TiAl(2.4952) / UNS N07080/ BS 3HR1(Nimonic 80A / NiCr20TiAl(2.4952) / UNS N07080/ BS 3HR1 Datasheet and Material certificate)

Product Details

GE spec NB 00146, Ideally released to GE spec NB 00146 or  to ASTM B637 or WK 2.4952 or BS 3HR1, VIM+ESR, Hot Forging,Polishing,

Grade

2.4952

Nimonic 80A

C

0.04~0.10

≤0.10

Si

≤1.00

≤1.00

Mn

≤1.00

≤1.00

P

≤0.020

—

S

≤0.015

≤0.015

Ni

≥65.00

Balance

Cr

18.00~21.00

18.00~21.00

Ti

1.80~2.70

1.80~2.70

Al

1.00~1.80

1.00~1.80

Co

≤1.00

≤2.00

Fe

≤1.50

≤3.00

Cu

≤0.20

≤0.20

B

≤0.008

≤0.008

Zr

—

≤0.15

Pb

—

≤0.0025


Related Products